Sketch-framed title card for glass countersinking

Countersunk Holes in Glass: Design, Specification and Machining

A countersunk hole in glass is a cylindrical through-hole with a conical recess at its mouth, so that a flat-head fastener sits flush with, or just below, the glass surface. It can be made reliably, but glass punishes the habits that work in metal: the cone must match the fastener, the hole must be placed away from edges, and the glass must be machined before it is toughened. We machine technical glass to drawing at Precision Glasses, and this guide sets out what an engineer needs on the drawing to get a part that fits, passes inspection and does not crack in service.

Precision Glasses
glassprecision.com
Specify Glass Holes With Confidence
Precision Glasses designs, fabricates, and supplies custom glass components for demanding applications, including parts machined to drawing.

Visit

TL;DR

  • A countersink is the conical recess, a counterbore is a flat-bottomed step. The cone angle is set by the fastener, not by the thread diameter.
  • Metric flat-head fasteners normally use a 90° cone and imperial ones 82°, so confirm the screw standard before the drawing is released.
  • Machine the countersink before toughening: toughened glass cannot be drilled or ground afterwards without breaking.
  • Keep holes well away from edges, corners and each other, and let the fixing allow for movement, because stress concentrates at the hole.
  • Give the supplier the full callout: clearance diameter, countersink major diameter, included angle, head position and tolerances.

Table of Contents

Countersink, counterbore and countersunk hole: the terms

The terms are used loosely, so a drawing needs to be exact. A countersink is the conical cutter or the conical recess it leaves. A countersunk hole is the whole feature: a straight clearance hole with that cone coaxial to it. A counterbore is different: a larger, flat-bottomed cylindrical recess, used where a socket-head cap screw or a washer needs a square seat. The Wikipedia entry on countersinking gives the same split between a conical and a flat-bottomed recess.

Glass samples showing conical and flat recesses

In glass, the choice between them is driven by load path. A cone gives a flush finish and a self-centring seat for a flat-head screw. A counterbore gives a flat seat that suits a gasket, bush or washer. For display covers, instrument windows and lighting lenses, where the front face must be clean, the countersink is the usual answer. The cost is that a cone puts a sharp-edged conical wall into a brittle material, which is why the details below matter.

When countersunk holes are the right choice

Countersunk holes appear wherever glass is screwed to a frame, bezel or housing and the outer face must be flat:

  • Automotive dashboards and touch screen covers, where the glass sits flush within a trim line.
  • Aerospace and defence instrument panels, where a protruding head would snag, reflect light or break the seal.
  • Medical device housings, where a smooth surface is easier to clean.
  • Marine and maritime displays, where a flat face sheds water and withstands washdown.
  • Lighting lenses and scanner glass, where fixing hardware must not interrupt the optical surface.

A flush head is not always the right call. If the glass is thin, the cone leaves very little parallel wall under it. As a rule of thumb, the thinner the glass, the more a counterbore, a bonded fixing or a clamp is worth considering. The decision belongs in the design review, before the glass thickness is frozen.

Choosing the angle: let the fastener decide

The cone angle is determined by the fastener that will sit in it. The GD&T Basics entry on countersinks notes that metric fasteners use a 90° countersink and imperial fasteners an 82° one. So the first question for any drawing is which screw standard the assembly uses.

Two errors recur:

  1. Choosing the angle from the thread size. The thread diameter says nothing about the head’s included angle. Take the angle from the fastener specification.
  2. Mixing 90° and 82° parts. An 82° screw in a 90° cone bears on a thin ring near the edge of the cone instead of across the surface. In metal that is untidy. In glass it concentrates load on the sharpest part of the feature.

A flat-head screw does not bear on glass directly in a well-designed assembly. A bush, grommet or washer with a matching cone (often plastic or a soft metal) sits between metal and glass, so that the load is spread and there is no metal-to-glass contact. This is the norm in point-supported glazing, and it applies equally to small precision parts.

What belongs on the drawing

A countersunk hole in glass should be specified with a full callout rather than a single symbol. Include:

ItemWhy it matters
Clearance-hole diameter and toleranceSets the gap around the shank; too tight and thermal or assembly movement loads the glass
Countersink major diameter and toleranceControls how far the head sits below or above the surface
Included angle (90° or 82°)Must match the fastener
Required head position (flush, below by a stated amount)Fixes the cone depth and the remaining parallel wall
Hole position from datum edgesControls fit to the housing; see edge distances below
Edge finish on the hole and coneChamfered or polished edges reduce the starting points for cracks
Surface-quality and chip limitsDefines what counts as acceptable chipping at the rim
Toughening state and sequenceTells the supplier the machining must come first

The GD&T Basics example shows the standard pattern: a through-hole diameter with tolerance, then a countersink diameter with tolerance and a conical angle. Add, for glass, the surface-quality and edge requirements. For tolerance schemes that suit glass rather than metal, our guide to GD&T and ISO 10110 for glass explains how to avoid rework from mismatched callouts.

A worked example: a 6 mm toughened cover with M4 metric flat-head screws. The clearance hole is drawn at a diameter that leaves a clear gap around the shank, the cone is 90°, the major diameter is set so the head or bush sits flush, and the cone depth is checked to be well under the glass thickness so a parallel wall remains below it. The numbers come from the screw standard and the bush you choose, not from a generic table, which is why we ask for the fastener drawing with the glass drawing.

Placement: edges, corners and spacing

A hole interrupts the stress field in the glass, and the countersink cone adds a sharp internal geometry. Both raise local stress. Placement therefore carries as much weight as the hole itself.

  • Edge distance. Keep the hole rim well away from the nearest edge. Fabricators commonly work to a multiple of the glass thickness, and the figure that applies to your part should be agreed with the supplier and written on the drawing.
  • Corner distance. Holes near corners are the highest-risk positions, since two edges and a hole combine.
  • Hole-to-hole spacing. Closely spaced holes share a stress zone. Keep adequate land between the rims.
  • Cone depth against thickness. The cone removes glass. Leave a parallel wall that is a meaningful proportion of the thickness.

For very small holes the rules change again, because the process changes: see our guide to micro hole drilling in glass for methods, limits and specifications at that scale.

Toughening, annealed and chemically strengthened glass

The order of operations is the most common cause of scrap with this feature. Fully toughened (thermally tempered) glass holds a high compressive layer at the surface balanced by tension in the core. Cut or grind through that layer and the stored energy is released as the glass breaks into small pieces. So every hole, countersink, notch and edge finish is completed first, and toughening is the last step. Our guide to what toughened glass is and how it behaves covers the process, and the page on annealed glass explains why annealed material is the base state for machining.

Two consequences for the designer:

  1. Thermal toughening changes geometry slightly. Holes and edges can distort in the furnace, so tolerances after toughening are wider than after machining. State which condition each tolerance applies to.
  2. Chemically strengthened glass is an alternative for thin parts or tight flatness, since the process is ion exchange rather than rapid cooling. The chemically strengthened glass guide sets out when it suits an engineered part.

Stress at the hole: figures worth knowing

The Glass Association of North America’s bulletin on point-supported glazing (FB07-05) refers to allowable stress limits at hole positions of 9,700 psi (67 MPa) for fully tempered glass and 3,500 psi (24 MPa) for heat-strengthened glass, citing ASTM C1048. These figures come from architectural glazing, so treat them as an order-of-magnitude guide for small instrument parts rather than a pass mark. The ratio is the useful part: fully tempered glass tolerates nearly three times the stress at a hole that heat-strengthened glass does.

Stress limits compared for two glass types

The same bulletin notes that when the glass deflects laterally by more than half its thickness, linear calculations stop being valid and non-linear plate theory is needed, often with finite element analysis for tempered or laminated glass. For a thin display cover under pressure, such as a marine or aerospace panel, check the deflection early. If you are near that threshold, model the hole and cone region explicitly.

Allow the glass to move

Most cracks at a countersunk hole in service do not come from machining. They come from the fixing forcing movement into the glass. The point-supported glazing bulletin says the movement capabilities and limits of hardware connections must be considered, and that oversized holes or slotted connections can allow for glass movement. The German standard DIN 18008-3, which covers point-supported glazing, takes the same line: the hardware must be able to compensate for structural deflection, or movement ends in fracture at the hole.

In practice:

  • Use a bush or washer between metal and glass so there is no hard contact.
  • Do not over-torque. Specify a torque or use a spring or compliant element where the assembly sees temperature swings.
  • Where housing and glass have different thermal expansion, use clearance holes sized for the movement, or slots. Our guide to glass slot machining covers that option.
  • Check thermal gradients. Our note on thermal shock limits in glass explains why edge and hole conditions matter when parts heat unevenly.

How countersunk holes are machined in glass

The process is not drilling and countersinking as in metal. Glass is ground away by diamond tooling with coolant, and the process is built to avoid chipping on the entry and exit faces.

A typical sequence on a CNC machine:

  1. Locate and secure the glass on a vacuum or supported fixture, referenced to the datum edges.
  2. Drill the through-hole with a diamond core drill or ultrasonic tool, with continuous coolant. Light, steady feed matters: LiteSpec’s guidance on drilling glass warns that excessive force chips the entry and exit faces.
  3. Form the cone with a diamond countersink tool or by interpolated grinding, working to the specified major diameter and angle.
  4. Finish the edges of the hole and cone to the drawing, typically with a chamfer or polish.
  5. Inspect dimensions, angle and rim chipping against the drawing before the glass goes to toughening, coating or printing.

Our pages on ultrasonic drilling of glass and CNC glass machining describe how these methods work and where each is specified. For a broader view of the sequence, see the explanation of glass machining for engineers.

Where it goes wrong

  • Chipping at the exit face, from excess feed or an unsupported back face.
  • Cone not concentric with the hole, which leaves the screw off-centre and loads one side.
  • Cone too deep, leaving a thin parallel wall.
  • Sharp, unfinished cone edges, which act as crack starters and show up later as failures in service or in thermal cycling.
  • Coating and printing applied over a damaged edge, which hides the defect until it grows.

Sequence with coatings, printing and lamination

Holes interact with the other processes on the same part. Ceramic printing is normally applied to the finished-shape glass, so the hole and cone must be final before it. Anti-reflective or anti-glare coatings go on the final geometry too, and the cone needs masking or a defined coating boundary if the fastener will touch it. For laminated parts, a hole through two plies needs the plies aligned closely, and the interlayer must be considered at the cone. Our guide to laminated display glass covers specification for those assemblies.

Put the order on the drawing or in the process note: cut, machine, edge finish, inspect, toughen, print, coat, assemble. A supplier who sees the sequence can plan around it. A supplier who does not may toughen first.

Perspective

Every month we see the same pattern in glass drawings: the countersink is drawn as in a metal bracket, with a symbol and a screw size, and nothing else. For glass that is not enough. The cone, the clearance hole, the edge finish and the toughening sequence all have to be stated, because they decide whether the part survives assembly.

Our view is that the cheapest place to fix a countersunk hole is on the drawing. We work through ISO 9001 certified, traceable production, with batch-level traceability, and we scale from prototype to volume, so the specification you validate on a first run is the one carried into production. Quality control and advanced inspection are part of that process, because a hole that was not checked before toughening cannot be corrected after.

If your part has a countersunk hole, send us the fastener drawing together with the glass drawing. Matching the two early is what keeps a programme out of rework.

Alexandra

Specifying countersunk glass parts with Precision Glasses

We design, fabricate and deliver custom glass components for medical devices, defence, aerospace, automotive dashboards, lighting, electronics, and marine and maritime technology. Our CNC glass machining and related services cover glass cutting, edge finishing, toughened and laminated glass, coated glass and display glass, with documented export compliance for regulated programmes. Send the drawing with the fastener specification and the application, and we will work through the callout with you before production.

Precision Glasses

For optical parts that also need holes or mounting features, our optical components range and technical glass pages show what we supply.

FAQ

What is the difference between a countersink and a countersunk hole?

A countersink is the conical recess, or the tool that cuts it. A countersunk hole is the complete feature: the straight through-hole with the cone at its mouth. On a drawing, the callout describes both, so give the clearance diameter, cone diameter and angle together.

Are countersinks always 45 degrees?

No. The angle given for a countersink is usually the included angle, and it is set by the fastener. Metric flat-head screws normally take 90° and imperial ones 82°, according to GD&T Basics. Half-angles of 45° and 41° follow from those figures.

Can you countersink toughened glass after toughening?

No. Toughened glass breaks when its surface compression layer is cut, so holes, countersinks and edge work are done first and toughening last. If a change is needed after toughening, the part is remade, which is why the drawing should be frozen before the glass is released.

How do I choose the countersink dimensions for my glass thickness?

Start from the fastener or bush: its head angle and head diameter set the cone angle and major diameter. Then check that the cone depth leaves a parallel wall in the glass thickness, and that the hole is placed well clear of edges and corners. Confirm the figures with your glass supplier against the specific thickness and toughening state.

Sources

Share

Leave a Reply

Your email address will not be published. Required fields are marked *

✅

Message Sent!

Thank you for contacting us.
We'll get back to you shortly.